Leather and a method of dressing same
US6610368B2 · kind B2 · utility
3Cited by
16References
9Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Mar 29, 2001 |
| Grant date | Aug 26, 2003 |
| Priority date | — |
| Expiry date | Mar 29, 2021 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC14C11/00
- WIPO fieldSurface technology, coating
- WIPO sectorChemistry
Abstract
Tanned leather is dry dressed by plasma deposition at atmospheric pressure of a matrix material such as ITO, a silicone, or polyurethane, upon the protein fibers of the surface of the leather and the collagen fiber skeleton below the surface protein fibers. The leather retains its toughness, elasticity, breathability and softness or hand.