Extrusion method utilizing maximum exit temperature from the die
US6630039B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Feb 14, 2001 |
| Grant date | Oct 7, 2003 |
| Priority date | — |
| Expiry date | Feb 14, 2021 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC22F1/05
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A method of producing an aluminum base alloy extruded product. The method comprises (a) providing a body of an aluminum base alloy; (b) homogenizing the body at an elevated temperature not exceeding its eutectic temperature for a sufficient period of time to provide a homogeneous distribution of the readily soluble alloy elements, (c) rapidly cooling the body; (d) reheating the body to a reheat temperature of at least 700° F. for a period of at least 0.5 hours; (e) extruding the body from the reheat temperature; (f) solution heat treating the body; and (g) quenching and aging the body.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.