Patent · US Expired

Powder core and reactor using the same

US6646532B2 · kind B2 · utility

3Cited by
2References
7Claims
0Family size

Assignee

Inventors

Key dates

Filing dateFeb 26, 2002
Grant dateNov 11, 2003
Priority date
Expiry dateApr 15, 2022

Classification

  • Technology area (CPC H)Electricity
  • CPC primaryH01F17/062
  • WIPO fieldElectrical machinery, apparatus, energy
  • WIPO sectorElectrical engineering

Abstract

Preparation is made of alloy powder comprising 3.0-8.0 wt % Si, 0.1-1.0 wt % O, 0-2.0 wt % (0 being exclusive) of at least one element selected from Mn, Al, V, Cr, and Ti, and balance Fe and having a particle size substantially equal to 150 &mgr;m or less. A binder is mixed with the alloy powder to form a mixture. The mixture is compaction-formed by the use of a die. Thus, a powder core is obtained which has a 20 kHz a.c. permeability equal to 20 or more under an applied d.c. magnetic field of 12000 A/m, a core loss characteristic of 1000 kW/m3 under the conditions of 20 kHz and 0.1 T, saturation magnetization of 10000 G or more, and coercive force of 3.0 Oe or less.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.