The bodies are prepared either by pelleting of a pasty mixture of titanium dioxide powder and titanium dioxide sol and/or 1-20% nitric acid, followed by dehydration and calcination at a temperature of between 400 and 1000° C. for between 0.5 and 3.5 hours; or by preparing pellets from the titanium dioxide powder and added water, annealing of the pellets at between 300 and 500° C., saturation of same with titanium dioxide sol or 1-20% nitric acid in a vacuum, followed by drying and finally annealing at a temperature of between 400 and 1000° C. for between 0.5 and 3 hours.