Patent · US Expired

Fiber-composite material and a method for producing the same

US6673452B1 · kind B1 · utility

3Cited by
3References
17Claims
0Family size

Assignee

Inventors

Key dates

Filing dateApr 19, 2002
Grant dateJan 6, 2004
Priority date
Expiry dateApr 19, 2022

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/31525
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

The invention relates to the field of chemistry and to a fiber composite material which is used, for example, in aircraft. The invention provides a fiber composite material in which delamination can be significantly reduced. This is achieved by a fiber composite material with multiple layers, each containing a duromer matrix and reinforcing fibers, inner layers contain fibers featuring a high level of adhesion to the duromer matrix, outer layers contain fibers featuring a low level or no adhesion to duromer matrix. There is also provided a method in which the reinforcing fibers include a coating and the layers are structured in such a way that, on the interior of the fiber composite material, layers are arranged which contain fibers with a high level of adhesion to the duromer matrix and that outer layers which contain fibers with a lower or low level of adhesion, or no adhesion to the duromer matrix are arranged on and/or around these inner layers.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.