Magnetic acicular alloy particles containing iron as a main component
US6682813B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Jul 17, 2002 |
| Grant date | Jan 27, 2004 |
| Priority date | — |
| Expiry date | Jul 17, 2022 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10T428/2982
- WIPO fieldElectrical machinery, apparatus, energy
- WIPO sectorElectrical engineering
Abstract
Magnetic acicular alloy particles containing iron as a main component according to the present invention, have an average major axial diameter of 0.05 to 0.2 &mgr;m, and pH values of water suspensions of said magnetic acicular alloy particles containing iron as a main component, which satisfies the formula:(pH value of water suspension treated by A method)−(pH value of water suspension treated by B method)<0 Such magnetic acicular alloy particles containing iron as a main component exhibit an excellent dispersibility in a vehicle, especially such a vehicle composed of a binder resin having a polar group such as —SO3M (wherein M is H, Na or K), —COOH or the like, and in which an orientation and a packing density in coating film are improved.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.