Patent · US Expired

Sulfoaluminous clinker without iron and without free lime, its process of preparation and its use in white binders

US6695910B2 · kind B2 · utility

11Cited by
12References
17Claims
0Family size

Assignee

Inventors

Key dates

Filing dateOct 24, 2002
Grant dateFeb 24, 2004
Priority date
Expiry dateOct 24, 2022

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02P40/10
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

The lightly colored sulfoaluminous clinker contains: more than 55% by weight of calcium sulfoaluminate phase (C4A3S), more than 10% by weight of belite phase (C2S), less than 10% by weight of anhydrite (C{overscore (S)}), and contains practically no ferrite phase, nor a gehlenite phase (C2AS), nor free lime. It is prepared by a process of roasting carried out at temperatures comprised between about 1250° C. and 1350° C. It can be used for a wide range of applications by combining it with a source of calcium sulfate and/or Portland cement, to obtain binders having specific properties (color, setup time, mechanical strength, expansion or contraction . . . ).