Process for synthesizing noncrystalline lithium based mixed oxides by high energy milling
US6713037B2 · kind B2 · utility
Assignee
Inventor
Key dates
| Filing date | Sep 30, 2002 |
| Grant date | Mar 30, 2004 |
| Priority date | — |
| Expiry date | Sep 30, 2022 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC01P2004/64
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A process method for producing a lithium based mixed oxide of the formula LiM′x . . . Oy through the steps of combining a lithium oxide with a second oxide having the base metal element (M′) at room temperature; and applying to the combination, a high energy milling process, wherein the high energy milling process obtains, without the addition of substantial external heat being added to the synthesis, a chemical synthesis of a composite oxide of the above formula, having crystallites of nanometer dimension.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.