Quenching a work piece made of a titanium alloy having a temperature higher than 800° C. to a temperature lower than 500° C. at a cooling rate greater than 10° C./second between 800° C. and 500° C. is used to render the cooled work piece containing &agr;″ phase as a major phase. The work piece is preferably a medical implant.