Preparation of polyethylene
US6727331B2 · kind B2 · utility
1Cited by
11References
8Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Dec 28, 2001 |
| Grant date | Apr 27, 2004 |
| Priority date | — |
| Expiry date | Mar 5, 2022 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08F110/02
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
A polyethylene having improved rheological properties is disclosed. The polyethylene has a melt index (MI2) from about 0.01 dg/min to about 50 dg/min and a melt strength (&eegr;) that satisfies MI2×&eegr;≧3.5. A process for making the polyethylene is also disclosed. The process uses an azaborolinyl-containing single-site catalyst in the presence of hydrogen, where the hydrogen consumption is controlled to be less than 30%.