Perfluoroelastomers having a low glass transition temperature and method of making them
US6730760B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Dec 11, 2001 |
| Grant date | May 4, 2004 |
| Priority date | — |
| Expiry date | Dec 11, 2021 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08F14/26
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
A method of making a curable fluoroelastomer is disclosed. The method comprises the steps ofpreemulsifying at least one perfluorovinylether in water, andcopolymerizing the preemulsified perfluorovinylether with a gaseous fluorinated monomer in the presence of a cure site monomer. The method provides a fluoroelastomer having a glass transition temperature of less than −10° C. Also disclosed is a fluoroelastomer that consists essentially of a perfluorovinylether of formula (I) as defined below, a cure site component, perfluoromethylvinylether, and tetrafluoroethylene and/or chlorotrifluoroethylene.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.