Method for producing nickel hydroxides
US6752918B1 · kind B1 · utility
1Cited by
3References
10Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Nov 5, 2001 |
| Grant date | Jun 22, 2004 |
| Priority date | — |
| Expiry date | Nov 5, 2021 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02E60/10
- WIPO fieldSurface technology, coating
- WIPO sectorChemistry
Abstract
A process is described for the production of spherical nickel hydroxide by anodic dissolution of a nickel electrode and precipitation of nickel hydroxide in a completely intermixed electrolysis cell, wherein an electrolysis brine is used which has a content of 20 to 50 g/l of chloride ions and 1 to 7 g/l of ammonia with a pH value of 9.5 to 11.5 and a temperature of 45 to 60° C.