Glassy-crystalline material with low solubility and process of preparing the same
US6767854B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Jun 13, 2002 |
| Grant date | Jul 27, 2004 |
| Priority date | — |
| Expiry date | Jun 26, 2022 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC03C10/16
- WIPO fieldMedical technology
- WIPO sectorInstruments
Abstract
The invention refers to a material which is chemically long-term stable in a neutral or slightly acid environment and which can be used both as bioactive bone replacement material, e.g. in the form of a coating applied onto metallic prosthesis sticks by thermal spraying, and as substrate material in biotechnology, e.g. in the form of a ceramic sheet. According to the invention, said material comprises 15-45% by weight CaO, 40-45% by weight P2O5, 10-40% by weight ZrO2 and fluoride, said material further comprises two crystalline phases being apatite and calcium zirconium phosphate, and a secondary glass phase. Said material has a very high chemical long-term stability, compared to known materials which can also be produced by means of a melting process.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.