Method of making an optical fiber using preform dehydration in an environment of chlorine-containing gas, fluorine-containing gases and carbon monoxide

US6776012B2 · kind B2 · utility

3Cited by
14References
17Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJun 26, 2001
Grant dateAug 17, 2004
Priority date
Expiry dateNov 6, 2021

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02P40/57
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

Embodiments of the invention include a method for making optical fiber having reduced aging or hydrogen aging loss over the life of the fiber and optical fiber systems including such optical fibers. The method includes the steps of dehydrating an optical fiber glass core rod in a first environment including oxygen and at least one of chlorine-containing gases, fluorine-containing gases and carbon monoxide; and adjusting the oxygen stoichiometry of the first environment so that it is neither oxygen-rich nor oxygen-deficient. Improved silicon-oxygen stoichiometry during one or more preform manufacturing steps reduces the amount of Si defects generated in the optical fiber preform. Also, deuterium exposure of optical fiber drawn from the preform reduces the likelihood of having atomic defects such as Si defects in the optical fiber that, over time, attract and bond with hydrogen atoms to form molecules that contribute to increased water absorption loss. The inventive method produces optical fibers with improved transmission characteristics, e.g., optical fibers made by methods according to embodiments of the invention have transmission loss at 1385 nanometers that is less than 0.33 dB…