Patent · US Expired

Method and device for manufacturing a hot rolled steel strip

US6776857B2 · kind B2 · utility

13Cited by
1References
11Claims
0Family size

Assignee

Inventor

Key dates

Filing dateAug 26, 2002
Grant dateAug 17, 2004
Priority date
Expiry dateOct 1, 2022

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC21D8/0263
  • WIPO fieldMachine tools
  • WIPO sectorMechanical engineering

Abstract

The present invention provides an effective method for mechanically removing iron oxide films formed on the surfaces of a hot rolled steel strip with a high temperature. The method comprises the steps of: maintaining a steel strip coil at a high temperature of 400° C. or more until the phase transformation is completed, after hot rolling; water-cooling the steel strip coil at a speed of at least 50° C./sec to 100° C. or less while uncoiling the coil; correcting the shape of the steel strip using a correction rolling mill; removing oxide films formed on surfaces of the shape-corrected steel strip by injecting water jets to the surface; and drying the steel strip free of oxide films and winding the steel strip. Also, the present invention provides an apparatus for carrying out this method.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.