Patent · US Expired

Method for producing through extrusion an anisotropic magnet with high energy product

US6787083B2 · kind B2 · utility

0Cited by
2References
5Claims
0Family size

Assignee

Inventor

Key dates

Filing dateSep 26, 2002
Grant dateSep 7, 2004
Priority date
Expiry dateMar 29, 2023

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T29/49076
  • WIPO fieldOther special machines
  • WIPO sectorMechanical engineering

Abstract

A method for producing an anisotropic magnet with high energy product through extrusion and, more specifically, by placing a particle charge of a composition from the which magnet is to be produced in a noncircular container, heating the container and particle charge and extruding the container and particle charge through a noncircular extrusion die in such a manner that one of the cross-sectional axes or dimension of the container and particle charge is held substantially constant during the extrusion to compact the particle charge to substantially full density by mechanical deformation produced during the extrusion to achieve a magnet with anisotropic magnetic properties along the axes or dimension thereof and, more specifically, a high energy product along the transverse of the smallest cross-sectional dimension of the extruded magnet.