Process for the production of low-molecular-weight allylamine polymer or addition salt thereof
US6787587B1 · kind B1 · utility
Assignee
Inventors
Key dates
| Filing date | Apr 12, 2000 |
| Grant date | Sep 7, 2004 |
| Priority date | — |
| Expiry date | Apr 12, 2020 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08F6/003
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
Disclosed are a process for the production of a low-molecular-weight allylamine polymer having a weight average molecular weight of 250 to 4,000 or an addition salt thereof, which comprises distilling a low-molecular-weight allylamine polymer solution to distill off unreacted monoallylamine, then, subjecting a residue to electrodialysis, and optionally carrying out acid treatment, a low-molecular-weight allylamine polymer having an ignition residue content of 5% by weight or less and a weight average molecular weight of 250 to 4,000, or an addition salt of a low-molecular-weight allylamine polymer having said properties, a water-resistance-imparting agent for use in an ink which comprises the above polymer or addition salt, and an ink composition comprising a colorant and the above water-resistance-imparting agent.According to the process of the present invention, a low-molecular-weight allylamine polymer improved in coloring and almost free of an inorganic salt or an addition salt thereof can be efficiently obtained. Further, the ink composition comprising the low-molecular-weight allylamine polymer or the salt thereof, provided by the present invention, not only has high water re…
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.