Patent · US Expired

Epoxidized polyalkenylenes and method for their preparation

US6797787B2 · kind B2 · utility

10Cited by
3References
16Claims
0Family size

Assignee

Inventors

Key dates

Filing dateDec 19, 2002
Grant dateSep 28, 2004
Priority date
Expiry dateJan 20, 2023

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC08C19/06
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

An epoxidized polyalkenylene is prepared reacting a polyalkenylene, an aqueous solution of 15 to 90% by volume of hydrogen peroxide and a carboxylic acid having from 1 to 3 carbon atoms in the presence of a catalyst which is phosphonic acid, a derivative of phosphonic acid or a mixture thereof, without addition of an organic solvent or water, to obtain the epoxidized polyalkenylene. The epoxidized polyalkenylene has a number-average molar mass of between 500 and 50 000 g/mol and an epoxide oxygen content of between 1 and 25 percent by mass.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.