Cold rolled steel

US6841010B2 · kind B2 · utility

0Cited by
1References
18Claims
0Family size

Assignee

Inventors

Key dates

Filing dateDec 26, 2002
Grant dateJan 11, 2005
Priority date
Expiry dateDec 26, 2022

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC21D8/0236
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A steel strip is produced having a tensile strength of at least 680 MPa but is such that the total elongation to break off of the strip after annealing is in the range 9% to 12%. Cold rolling may produce a cold reduction of the strip thickness in the range 40% to 80%. The continuously cast strip may be optionally in-line hot rolled prior to coiling to produce an initial strip thickness in the range 40% to 60%.