Patent · US Expired

Hot working die steel excelling in molten corrosion resistance and strength at elevated temperature and member for high temperature use formed of the hot working die steel

US6841122B2 · kind B2 · utility

0Cited by
3References
11Claims
0Family size

Assignee

Inventors

Key dates

Filing dateApr 29, 2002
Grant dateJan 11, 2005
Priority date
Expiry dateApr 29, 2022

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC21D1/06
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A hot working die steel contains 0.05-0.25% C, 0.30% or less Si, 0.03% or less Mn, 1.0% or less Ni, 5.0-13.0 % Cr, 2.0% or less Mo, 1.0-8.0% W, 1.0-10.0% Co, 0.003-0.020% B, 0.005-0.050% N, and the balance consisting essentially of Fe and unavoidable impurities. If desired, the hot working die steel may further contain 0.01-1.0% V and 0.01-1.0% of at least one kind selected from Nb and Ta.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.