Patent · US Expired

Method using selected carbons to react with Al2O and Al vapors in the carbothermic production of aluminum

US6849101B1 · kind B1 · utility

6Cited by
8References
12Claims
0Family size

Assignees

Inventors

Key dates

Filing dateDec 4, 2003
Grant dateFeb 1, 2005
Priority date
Expiry dateDec 4, 2023

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22B21/02
  • WIPO fieldChemical engineering
  • WIPO sectorChemistry

Abstract

In a method for recovering Al from an off-gas (3,4) produced during carbothermic reduction of aluminum utilizing at least one smelter (1,2), the off-gas (3,4) is directed to an enclosed reactor (5) which is fed a supply of wood charcoal (7) having a porosity of from about 50 vol. % to 85 vol. % and an average pore diameter of from about 0.05 μm to about 2.00 μm, where the wood charcoal (7) contacts the off-gas (3,4) to produce at least Al4C3 (6), which is passed back to the smelter (1,2).

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.