Method for producing polybutadiene latex with an optimized thermal current profile
US6852797B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Apr 24, 2001 |
| Grant date | Feb 8, 2005 |
| Priority date | — |
| Expiry date | Apr 24, 2021 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10S525/942
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
A polybutadiene latex is prepared by a process in which butadiene is polymerized by free radical emulsion polymerization in the presence of initiator and, if required, dispersants and further conventional assistants, the polymerization being carried out in the presence of reactive comonomers in such a way that the heat flow of 43 watt/kg solids content of the polymerization mixture is not exceeded. Owing to the presence of reactive comonomers, the reaction rate at the beginning of the reaction is increased, with the result that an overall flatter heat flow profile is obtained. A preferred reactive comonomer is styrene. Preferably, the process is carried out by a semi-batch procedure in which
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.