Patent · US Expired

Zirconium alloy highly resistant to corrosion and to sun burst by water and water vapor and method for thermomechanical transformation of the alloy

US6884304B1 · kind B1 · utility

12Cited by
2References
6Claims
0Family size

Assignee

Inventor

Key dates

Filing dateNov 21, 2000
Grant dateApr 26, 2005
Priority date
Expiry dateApr 28, 2021

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02E30/30
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

The alloy contains, by weight, at least 95% zirconium and from 0.01 to 0.1% sulphur and, optionally, at least one element from the group consisting of the elements tin, iron, chromium, hafnium, niobium, nickel, oxygen and vanadium, the balance of the alloy consisting of inevitable impurities. The sulphur is present in the alloy in the dissolved state, thereby improving the creep strength and in the form of uniformly distributed fine precipitates, thereby improving the corrosion and hydriding resistance. The alloy may be heated by a solution annealing treatment in the β phase followed by a quench or by a soak at a temperature below 950° C. in order to transform it into the α or α+β phase.