Method of producing pelletized polyolefin
US6894109B1 · kind B1 · utility
Assignee
Inventors
Key dates
| Filing date | Apr 1, 2003 |
| Grant date | May 17, 2005 |
| Priority date | — |
| Expiry date | Aug 1, 2023 |
Classification
- Technology area (CPC B)Performing Operations; Transporting
- CPC primaryB29K2023/12
- WIPO fieldOther special machines
- WIPO sectorMechanical engineering
Abstract
Rotational moulded products are prepared by producing a mixture of a polyolefin and optionally at least one additive, extruding this mixture in melt form through orifices in a die, pelletizing the mixture extruded through the orifices to form micropellets having a particle size distribution D(v, 0.5) of 0.1 to 1 mm, and a value of the ratio of D(v, 0.9)-D(v, 0.1) to D(v, 0.5) of no more than 1, drying the micropellets to a residual water content of no more than 1% weight, and if desired packaging the micropellets.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.