Rolled or extruded aluminium Al-Mn alloy products with improved corrosion resistance

US6896749B2 · kind B2 · utility

2Cited by
3References
11Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJan 9, 2002
Grant dateMay 24, 2005
Priority date
Expiry dateJan 9, 2022

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22C21/00
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

The invention concerns a rolled or extructed product, in particular a tube, made of an alloy composition (expressed in wt. %) comprising: Si<0.30; Fe 0.20-0.05; Cu<0.05; Mn 0.5-1.2; Mg<0.05; Zn<0.50; Cr 0.10-0.30; Ti<0.05; Zr<0.05; the balance consisting of aluminium and unavoidable impurities. The invention also concerns a method for making extruded tubes of said composition comprising casting a billet, optionally homogenizing it, extruding a tube, drawing said tube in one or several passes and continuous annealing at a temperature ranging between 350 and 500° C. with a temperature increase of less than 10 seconds. The inventive products are designed for pipes and heat exchangers for motor vehicles, and exhibit good corrosion resistance.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.