Abstract
A method for making reduced iron using blast-furnace sludge is provided. The method includes a mixing step of mixing the blast-furnace sludge and an iron-oxide-containing powder to prepare a mixed material, an agglomerating step of agglomerating the mixed material to form agglomerates, a feeding step of feeding the agglomerates onto a continuously moving hearth, and a reducing step of heating the agglomerates to remove zinc and reduce the agglomerates.