Patent · US Expired

Method of producing an abrasive product containing cubic boron nitride

US6919040B2 · kind B2 · utility

19Cited by
4References
47Claims
0Family size

Inventors

Key dates

Filing dateAug 3, 2001
Grant dateJul 19, 2005
Priority date
Expiry dateAug 3, 2021

Classification

  • Technology area (CPC B)Performing Operations; Transporting
  • CPC primaryB22F2005/001
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A method of producing an abrasive product consists of providing a mixture of a mass of discrete carbide particles and a mass of cubic boron nitride particles, the cubic boron nitride particles being present in the mixture in an amount such that the cubic boron nitride content of the abrasive product is 25% or less by weight, and subjecting the mixture to elevated temperature and pressure conditions at which the cubic boron nitride is crystallographically stable and at which substantially no hexagonal boron nitride is formed, in the presence of a bonding metal or alloy capable of bonding the mixture into a coherent, sintered product, to form the abrasive product. The bonding metal or alloy comprises a combination of a transition metal or a transition alloy and up to 40% by volume of the bonding metal or alloy of a second metal which is a stronger nitride or boride former than the transition metal or the transition metal alloy.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.