Recover and recycle rhodium from spent partial oxidation catalysts
US6923922B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Apr 21, 2004 |
| Grant date | Aug 2, 2005 |
| Priority date | — |
| Expiry date | Apr 21, 2024 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02P10/20
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A method for the recovery of rhodium from spent supported catalysts. In one embodiment, a method for recovering rhodium from a host material includes roasting the host material in air at a temperature sufficient to convert at least a portion of rhodium to Rh2O3, leaching the host material in a solution with a leaching constituent which is reactive with Rh2O3 to form a first intermediate species, reacting the first intermediate species in a solution with an acidifying constituent or complexing agent to form a second intermediate species, and purifying the second intermediate species. Preferably, the roasting temperature is approximately from 600° C. to 800° C. for 0.5 to 10 hours. In some embodiments, the host material is ground to particles in the range of 0.1 to 10 mm.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.