Catalysts with high cobalt surface area
US6927190B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Nov 9, 2004 |
| Grant date | Aug 9, 2005 |
| Priority date | — |
| Expiry date | Nov 9, 2024 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC07C2523/75
- WIPO fieldChemical engineering
- WIPO sectorChemistry
Abstract
A catalyst or precursor thereto comprising cobalt and/or a cobalt compound on a transition alumina support having a total cobalt content of at least 41% by weight and a cobalt surface area, after reduction, greater than 25 m2 per gram of total cobalt. The catalyst or precursor may be made by slurrying a transition alumina powder having a pore volume of at least 0.7 ml/g with an aqueous cobalt ammine carbonate complex and heating the slurry to decompose the complex.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.