Abstract
Reinforced high early-strength cementitious members are made from water and strength generating ingredients, which include a hydraulic cement, a polycarboxylate dispersant and structural synthetic fiber. The strength generating ingredients provide corrosion resistance by avoiding the use of steel reinforcing members, increased ductility and load bearing capacity while developing a high early-strength of at least about 1,400 pounds per square inch (psi) flexural strength and at least about 7,500 pounds per square inch (psi) compressive strength within about 24 hours after placing the cementitious composition in a mold.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.