Patent · US Expired

Method for making aluminum alloy strips with high surface homogeneity

US6948550B2 · kind B2 · utility

0Cited by
0References
15Claims
0Family size

Assignee

Inventors

Key dates

Filing dateDec 13, 2001
Grant dateSep 27, 2005
Priority date
Expiry dateJun 25, 2022

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC25D11/04
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A process for manufacturing a strip of aluminum alloy having high surface homogeneity with an upper side showing after a 1 μm thick sulphur anodic treatment, an optical roughness value SN measured on three 5 cm longitudinal sections and three 5 cm transverse sections, such that its mean variation on each section, defined by the ratio: (Maximum SN−minimum SN)/Mean SN is less than 20%, and the difference ΔSN=SN max −SN min is less than 20. The strip is manufactured by continuous casting between two cooled rolls from a casting tank containing the liquid metal connected to an injector, and feeding the liquid metal into the gap between the two rolls. The injector has an upper lip recessed by at least 2 mm with reference to a lower lip of the injector.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.