Molecular weight modification of thermoplastic polymers
US6949594B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | May 22, 2001 |
| Grant date | Sep 27, 2005 |
| Priority date | — |
| Expiry date | May 22, 2021 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08L2023/44
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
The invention relates to a process for the molecular weight increase/crosslinking of non-halogen-containing thermoplastic polymers, in which process a composition comprising a) a non-halogen-containing thermoplastic polymer; b) a functional compound having at least two unsaturated carbon bonds; and c) an alkoxyamine having a structural unit (I), which forms free radicals at the melting temperature/processing temperature of the polymer, is mixed and heated above the melting point of the polymer in the case of crystalline polymers or the softening point in the case of amorphous polymers. The invention relates also to the composition itself, to the use thereof in increasing the molecular weight of polymers and to polymers having increased molecular weight or crosslinked polymers prepared in accordance with that process
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.