Patent · US Expired

High temperature polyurethane/urea elastomers

US6964626B1 · kind B1 · utility

21Cited by
26References
33Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJun 12, 1996
Grant dateNov 15, 2005
Priority date
Expiry dateFeb 11, 2021

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10S528/906
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

The present invention relates to molded polyurethane/urea elastomers, and specifically to improved polyurethane/urea elastomers having high temperature stability to about 140–150° C. and low temperature flexibility at about −35–(−40)° C., for use in dynamic applications. These elastomers are particularly useful for application in belts, specifically in automotive timing or synchronous belts, V-belts, multi V-ribbed or micro-ribbed belts, flat belting and the like. The polyurethane/urea elastomers of the present invention are prepared by reacting polyisocyanate prepolymers with symmetric primary diamine chain extenders, mixtures of symmetric primary diamine chain extenders and secondary diamine chain extenders, or mixtures of symmetric primary diamine chain extenders and non-oxidative polyols, which are all chosen to eliminate the need for catalysts via standard molding processes, and to improve phase separation. The polyisocyanate prepolymers are reaction products of polyols which are nonoxidative at high temperatures, such as polycarbonate polyols, polyester polyols, or mixtures thereof, with organic polyisocyanates which are either compact, symmetric and aromatic, such as para-ph…

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.