Abstract
The invention is a method of bonding a ceramic part to a metal part by heating a component assembly comprised of the metal part, the ceramic part, and a compatible interlayer material such as titanium-nickel alloy placed between the two parts and heated at a temperature that is greater than the eutectic temperature of the interlayer material, where alloys, intermetallics or solid solution formed between the metal part and the metal interlayer material, but that is less than the melting point of either the ceramic part or the metal part. The component assembly is held in intimate contact at temperature in a non-reactive atmosphere for a sufficient time to develop a hermetic and strong bond between the ceramic part and the metal part. The bonded component assembly is optionally treated with acid to remove unwanted materials, to assure a biocompatible component assembly for implantation in living tissue.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.