High-temperature-resistant component and process for producing the high-temperature-resistant component
US7005015B2 · kind B2 · utility
12Cited by
4References
4Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Jan 29, 2002 |
| Grant date | Feb 28, 2006 |
| Priority date | — |
| Expiry date | Jan 29, 2022 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC30B29/52
- WIPO fieldSurface technology, coating
- WIPO sectorChemistry
Abstract
A high-temperature component made of a nickel super-alloy has the following composition in wt %: 11–13% of Cr, 3–5% of W, 0.5–2.5% of Mo, 3–5% of Al, 3–5% of Ti, 3–7% of Ta, 1–5% of Re and a remainder formed of nickel. A corresponding component which is also provided is formed of an alloy having a composition essentially similar to that mentioned above, but with the rhenium proportion replaced with 0.1–5 wt % of ruthenium.