Patent · US Expired

Material for shadow mask, method for production thereof, shadow mask comprising the material and picture tube using the shadow mask

US7026751B2 · kind B2 · utility

0Cited by
0References
4Claims
0Family size

Assignee

Inventors

Key dates

Filing dateNov 14, 2001
Grant dateApr 11, 2006
Priority date
Expiry dateJun 27, 2022

Classification

  • Technology area (CPC H)Electricity
  • CPC primaryH01J2229/0733
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A material for a shadow mask, characterized in that it has a chemical composition: C=0.0030 wt %, Si=0.03 wt %, Mn: 0.1 to 0.5 wt %, P=0.02 wt %, S=0.02 wt %, Al: 0.01 to 0.07 wt %, N=0.0030 wt %, B: an amount satisfying 0.5≦B/N≦2, and balance: Fe and inevitable impurities, and can form a shadow mask having a coercive force Hc of 90 A/m or less; and a method for producing the material, characterized in that use is made of a raw material having the above chemical composition, the finishing temperature in hot rolling is lower than Ar3 point by O to 30° C., the coiling temperature is 650 to 700° C., and the rolling reduction percentage in the final rolling (secondary cold rolling) is 30 to 45%. The material produced by the method exhibits magnetic characteristics being uniform in a coil and excellent as described above.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.