Cr-based alloy excellent in balance between strength and ductility at high temperature
US7037467B1 · kind B1 · utility
1Cited by
3References
6Claims
0Family size
Assignee
Inventor
Key dates
| Filing date | May 26, 2000 |
| Grant date | May 2, 2006 |
| Priority date | — |
| Expiry date | Jun 22, 2021 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC22F1/18
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A strength-ductility balance at a high temperature above 1000° C., particularly a high temperature above 1050° C. is improved by rendering a chemical composition of Cr-based alloy into Cr: not less than 60 mass %, C+N: not more than 20 mass ppm, S: not more than 20 mass ppm, O: not more than 100 mass ppm, O as an oxide: not more than 50 mass ppm, and the remainder being Fe and inevitable impurities.