High-temperature protection layer
US7052782B2 · kind B2 · utility
2Cited by
13References
11Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Jul 19, 2004 |
| Grant date | May 30, 2006 |
| Priority date | — |
| Expiry date | Jul 19, 2024 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10T428/26
- WIPO fieldSurface technology, coating
- WIPO sectorChemistry
Abstract
A high-temperature protection layer contains (% by weight) 23 to 27% Cr, 4 to 7% Al, 0.1 to 3% Si, 0.1 to 3% Ta, 0.2 to 2% Y, 0.001 to 0.01% B, 0.001 to 0.01% Mg and 0.001 to 0.01% Ca, remainder Ni and inevitable impurities. Optionally, the Al content is in a range from over 5 up to 6% by weight.