Patent · US Expired

Method for preparing pure, thermally stable and high surface area ceria

US7094383B2 · kind B2 · utility

10Cited by
7References
13Claims
0Family size

Assignee

Inventors

Key dates

Filing dateDec 14, 2004
Grant dateAug 22, 2006
Priority date
Expiry dateApr 7, 2025

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC01P2006/13
  • WIPO fieldChemical engineering
  • WIPO sectorChemistry

Abstract

A method for the preparing pure, thermally stable and high surface area ceria is described, wherein the ceria maintains a surface area of 12 m2/g after calcination at 980° C. in air for 4 hours. In the method, an aqueous solution containing Ce3+, Mg2+, organic acid and organic polymer is prepared and then evaporated to obtain a gel. The gel is calcined to obtain a mixed oxide, and then MgO is leached from the mixed oxide with a solvent to obtain raw ceria. The raw ceria is then washed, filtered and dried to obtain a ceria product.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.