High strength aluminum alloy

US7125459B2 · kind B2 · utility

3Cited by
21References
6Claims
0Family size

Assignee

Inventor

Key dates

Filing dateDec 21, 2004
Grant dateOct 24, 2006
Priority date
Expiry dateDec 21, 2024

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22F1/057
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A process for thermally treating an article made from an alloy comprising at least aluminum and copper. The process comprises solid solution heat treating the article, quenching the article, heating the article to a first temperature of from about 275 to about 340° F. and artificially aging. The article is artificially aged at the first temperature for a duration of at least 30 minutes. The article is artificially aged at a second temperature of from about 325 to about 380° F. for a duration of from about 4 hours to about 36 hours. The second temperature is greater than the first temperature by at least 10° F.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.