Patent · US Expired

Electroluminescent phosphor and its production method

US7135130B2 · kind B2 · utility

0Cited by
0References
3Claims
0Family size

Assignee

Inventors

Key dates

Filing dateFeb 10, 2004
Grant dateNov 14, 2006
Priority date
Expiry dateFeb 10, 2024

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC09K11/576
  • WIPO fieldBasic materials chemistry
  • WIPO sectorChemistry

Abstract

The invention provides electroluminescent phosphor having superior luminance and a long life. The host material is ZnS.aAO, of which “A” is at least one element selected from among magnesium (Mg), calcium (Ca), strontium (Sr), and barium (Ba). “a” ranges from 0.001 to 0.01. Either one of or both copper (Cu) or manganese (Mn) is contained as an activator. At least one element selected from among chlorine (Cl), bromine (Br), iodine (I), and aluminum (Al) is contained as a co-activator. The luminance and life span of the electroluminescent phosphor can be increased by limiting “a”, which represents the proportion of alkaline earth metal oxide (AO) introduced into the zinc sulfide, within the range of 0.001 to 0.01.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.