Dispersions of amorphous urethanized unsaturated polyester resins based on particular dicidol isomers
US7135522B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Dec 23, 2003 |
| Grant date | Nov 14, 2006 |
| Priority date | — |
| Expiry date | Nov 18, 2024 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08J2375/00
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
An aqueous dispersion, contains: a) an amorphous urethanized, unsaturated polyester resin, b) a nonvolatile content of from 20% to 60% by weight, c) from 0 to 60% by weight of a solvent, d) a pH of between 5.0 and 9.5, and e) a viscosity at 20° C. of from 20 to 500 mPas. The polyester resin is obtained from I. an alcohol component, II. i) from 20 to 100 mol % of an α,β-unsaturated carboxylic acid component, and ii) from 0 to 80 mol % of a further carboxylic acid component, and III. at least one isocyanate component. The alcohol component contains a dicidol mixture of the isomeric compounds 3,8-bis(hydroxymethyl)tricyclo[5.2.1.02,6]decane, 4,8-bis(hydroxymethyl)tricyclo[5.2.1.02,6]decane and 5,8-bis(hydroxymethyl)tricyclo[5.2.1.02,6]decane. Each isomer is present in a fraction of from 20 to 40% in the dicidol mixture. The sum of the three isomers in the dicidol mixture is from 90 to 100%. The dicidol mixture is present from 10 to 100 mol % in the alcohol component of the polyester.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.