Moderate temperature bending of magnesium alloy tubes
US7140224B2 · kind B2 · utility
9Cited by
17References
23Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Mar 4, 2004 |
| Grant date | Nov 28, 2006 |
| Priority date | — |
| Expiry date | Sep 28, 2024 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10S72/70
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A method for bending magnesium alloy tubes. The method includes heating the tube at moderate temperature in the range of about 100° C. to 200° C., and bending the tube to a bend angle or forming the tube to a desired shape.