Method for manufacturing a pressed part from a soft magnetic composite material
US7175794B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Feb 11, 2002 |
| Grant date | Feb 13, 2007 |
| Priority date | — |
| Expiry date | Oct 26, 2022 |
Classification
- Technology area (CPC B)Performing Operations; Transporting
- CPC primaryB22F2999/00
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A method for manufacturing a pressed part from a soft magnetic composite material. A starting mixture is provided that includes an iron powder and an auxiliary pressing agent. The starting mixture is pressed to form a pressed part and annealed at temperatures between 380° C. and 450° C. in a mixture of an inert gas and oxygen that has an oxygen concentration between 1% and 10% by volume. A second embodiment of a method for manufacturing a pressed part from a soft magnetic composite material in which a starting mixture is provided that includes an iron powder and an auxiliary pressing agent. The starting mixture is pressed to form a pressed part, annealed, and then postformed and re-annealed.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.