Casting of aluminum based wrought alloys and aluminum based casting alloys

US7201210B2 · kind B2 · utility

2Cited by
4References
19Claims
0Family size

Assignee

Inventors

Key dates

Filing dateDec 2, 2004
Grant dateApr 10, 2007
Priority date
Expiry dateDec 2, 2024

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22C1/02
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

Preferred embodiments of the present invention include methods that allow for casting alloys, and preferentially casting wrought alloys to circumvent problems such as, for example, hot tearing. Preferred embodiments of the present invention provide for alloys having predominantly spherical primary α-aluminum grains in their microstructure (i.e., substantially free of dendrites) formed by mixing two liquids of differing compositions that are held at predetermined temperatures, such that when mixed they produce a predetermined alloy composition at a predetermined temperature that is inclined to solidify with a predominantly spherical grain structure that minimizes the alloy's tendency towards hot tearing.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.