Patent · US Expired

Al-Cu-Li-Mg-Ag-Mn-Zr alloy for use as structural members requiring high strength and high fracture toughness

US7229509B2 · kind B2 · utility

30Cited by
3References
16Claims
0Family size

Assignee

Inventor

Key dates

Filing dateMay 26, 2004
Grant dateJun 12, 2007
Priority date
Expiry dateMay 26, 2024

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22C21/16
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

An improved aluminum lithium alloy comprising 0.1 to 2.5 wt. % Li, 2.5 to 5.5 wt. % Cu, 0.2 to 1.0 wt. % Mg, 0.2 to 0.8 wt. % Ag, 0.2 to 0.8 wt. % Mn, up to 0.4 wt. % Zr or other grain refiner such as chromium, titanium, hafnium, scandium or vanadium, the balance aluminum. The present alloy exhibits an improved combination of strength and fracture toughness, over any thickness range. The present invention is further directed to methods for preparing and using Al—Li alloys as well as to products comprising the same.