Patent · US Expired

Gamma prime phase-containing nickel aluminide coating

US7250225B2 · kind B2 · utility

6Cited by
4References
22Claims
0Family size

Assignee

Inventors

Key dates

Filing dateSep 26, 2005
Grant dateJul 31, 2007
Priority date
Expiry dateSep 26, 2025

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/12944
  • WIPO fieldSurface technology, coating
  • WIPO sectorChemistry

Abstract

An intermetallic composition suitable for use as an environmentally-protective coating on surfaces of components used in hostile thermal environments, including the turbine, combustor and augmentor sections of a gas turbine engine. The coating contains the gamma-prime (Ni3Al) nickel aluminide intermetallic phase and either the beta (NiAl) nickel aluminide intermetallic phase or the gamma solid solution phase. The coating has an average aluminum content of 14 to 30 atomic percent and an average platinum-group metal content of at least 1 to less than 10 atomic percent, the balance of the coating being nickel, incidental impurities, and optionally hafnium.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.