Method of making interpolymers and products made therefrom
US7271221B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Mar 21, 2005 |
| Grant date | Sep 18, 2007 |
| Priority date | — |
| Expiry date | Mar 21, 2025 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10S526/943
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
Olefin polymers having a melt strength of about 5cN at 190 ° C., and when made into a film have a CD shrink of at least 20%. Some of the polymers have a comb-like structure with at least 0.3 long-chain branches per 1000 carbon atoms are disclosed. Some compositions described herein include a high molecular weight fraction and a low molecular weight fraction wherein the ratio of the molecular weight of the high molecular weight fraction to the molecular weight of the low molecular weight fraction is greater than about 1.3.