Laminated ceramic capacitor

US7277268B2 · kind B2 · utility

6Cited by
9References
8Claims
0Family size

Assignee

Inventors

Key dates

Filing dateApr 16, 2004
Grant dateOct 2, 2007
Priority date
Expiry dateApr 16, 2024

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22C1/0433
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A metal alloy powder containing at least two alloying elements selected from the group of Ni, Cu, Cr, Sn, Mn, Co and W containing 1 to 99% by weight Ni, 1 to 99% by weight Cu, 6 to 60% by weight Cr, 6 to 15% by weight Sn, 6 to 15% by weight Mn, 6 to 15% by weight Co, and/or 6 to 15% by weight W for use in laminated ceramic capacitors with an internal electrode wherein said electrode comprises a sintered body of said alloy powder. A metal alloy powder containing at least two alloying elements selected from the group of Ni, Cu, Cr, Sn, Mn, Co and W wherein the onset of oxidation of the alloy powder occurs above about 250° C.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.