Method of making a hardened steel part, especially a roll load-bearing steel part
US7387694B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Oct 7, 2003 |
| Grant date | Jun 17, 2008 |
| Priority date | — |
| Expiry date | Nov 21, 2023 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC21D7/02
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
The method of making a hardened steel part or component includes making a semi-finished article of air-hardened steel; cold-forming the semi-finished article into a finished-shape part or component with a desired or predetermined finished shape and then hardening the finished-shape part or component with the finished shape by a heat treating process. The air-hardened steel particularly preferably contains about 0.67% by weight carbon, about 1.50 % by weight silicon, about 1.50% by weight manganese, about 1.00% by weight chromium, about 0.10% by weight nickel, about 0.25% by weight molybdenum, and a balance or remaining portion of iron with standard impurities.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.